01545А
Improved physical and mechanical properties of the alloy provides a balanced content of magnesium and scandium. This is due to the increase in strength characteristics.
Aluminum alloy 01545A belongs to the new generation of magnals of the second category. Due to the formation of dispersed aluminide particles, this material has greater ductility, strength, resistance to corrosion and fatigue than traditional aluminum-magnesium alloys. 01545A was successfully applied in the production of structures for racing cars, high-speed vessels, aircraft and spacecraft.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Sc, % | Si, % | Be, % | Mg, % | Mn, % | Cu, % | Zn, % | РЗЭ, % | V, % | Zr, % | Al, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 0.3 | 0.15–0.35 | < 0.3 | 0.0001–0.005 | 3.9–5.2 | 0.1–0.6 | < 0.3 | < 0.2 | < 0.004 | < 0.05 | 0.05–0.15 | 92.391–95.7999 | < 0.15 |
Information on suppliers
Mechanical properties at 20 °C
Analogues
| USA |
|---|
| A95025 UNS |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sc | % | Scandium |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| РЗЭ | % | Rare earth elements |
| V | % | Vanadium |
| Zr | % | Zirconium |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |