01H18N40M5GB-ID (EP753-ID)
The technological characteristic is corrosion resistance: the forged billet is tested for intergranular corrosion by a regulated method.
Forged pipes and pipe fittings for petrochemistry, for special equipment of nuclear power plants and for the needs of instrument-making are made of an alloy.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ni, % |
V, % |
Nb, % |
Mo, % |
N, % |
| TU 14-1-2097-77 |
51.085–55.2 |
< 0.1 |
1–2 |
39–41 |
0.05–0.2 |
0.25–0.6 |
4.5–5 |
< 0.015 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{0.2}$$, $$MPa$$ |
d5, % |
Treatment |
|
|
|
|
|
> 539 |
|
> 45 |
|
Mechanical properties at 1050 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{0.2}$$, $$MPa$$ |
d5, % |
Treatment |
|
|
|
|
|
|
196 |
|
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| d5 |
% |
Elongation at break |
| $$\sigma_{0.2}$$ |
$$MPa$$ |
Tensile stress required to produce a total elongation of 0.2% |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |