01H18N40M5GBR-ID (EP753R-ID)
The alloy is characterized by corrosion resistance and withstands tests by regulated methods.
Due to its properties, it is used in chemically aggressive environments in the form of forged pipes for special purposes in petrochemistry and in NPP equipment.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Ni, % | V, % | Nb, % | Mo, % | N, % |
|---|---|---|---|---|---|---|---|---|
| TU 14-1-2097-77 | 51.085–55.2 | < 0.1 | 1–2 | 39–41 | 0.05–0.2 | 0.25–0.6 | 4.5–5 | < 0.015 |
Information on suppliers
Mechanical properties at 20 °C
Standards
| Standard | Description |
|---|---|
| TU 14-1-2097-77 | TU 14-1-2097-77 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Ni | % | Nickel |
| V | % | Vanadium |
| Nb | % | Niobium |
| Mo | % | Molybdenum |
| N | % | Nitrogen |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |