02H15N60M16 (EP 367)
Advantages of the alloy:
- — heat resistance;
- — low temperature coefficient of expansion;
- — resistance to corrosion.
It has significant electrical resistance. Therefore, it is used in engineering, construction, energy. It has high heat-resistant properties.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | > 6.42 | < 0.5 | < 2 | < 15 | < 60 | < 0.03 | < 0.02 | < 0.03 | < 16 |
Information on suppliers
Casting and technological parameters
| melting point, °C | Hot working temperature, °C | annealing temperature, °C |
|---|---|---|
| 1400 | 1100 | 800 |
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
Description of the casting and technological parameters
| Parameter | Units of measurement | Description |
|---|---|---|
| melting point | °C | The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |
| Hot working temperature | °C | The temperature at which the plastic-deformed metal recrystallizes during the pressure treatment |
| annealing temperature | °C | The temperature at which the processes return recrystallization and homogenization of the metal to reduce its hardness for subsequent machining |