02Х25Н7М3
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Cr, % | Ni, % | C, % | Mo, % | N, % | PRE, % |
|---|---|---|---|---|---|---|---|
| GOST ISO 13680-2016 | 27.3 | 25 | 7 | 0.02 | 3 | 0.18 | 37.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST ISO 13680-2016 | |
| GOST R ISO 13680-2011 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| PRE | % | Pitting resistance |
| Cr | % | Chrome |
| Ni | % | Nickel |
| C | % | Carbon |
| Mo | % | Molybdenum |
| N | % | Nitrogen |