02Х27Н31М4 (HN30MDB-Sh)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Cr, % | Ni, % | C, % | Mo, % |
|---|---|---|---|---|---|
| GOST ISO 13680-2016 | 38.48 | 27 | 31 | 0.02 | 3.5 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| X1NiCrMoCu31-27-4 | 27-31-4 |
Standards
| Standard | Description |
|---|---|
| GOST ISO 13680-2016 | |
| GOST R ISO 13680-2011 |