03H13N9D2TM
for products operating at temperatures from +20 to -253 degrees.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Cryogenic structural steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1133-71 | 72.825–77.2 | < 0.5 | < 0.5 | 12–13 | 0.8–1.1 | 1.5–2 | 8–9 | < 0.02 | < 0.03 | < 0.025 | 0.5–1 |