03H18N16M3 (ZI133)
Sheet and long products, designed for the manufacture of surgical implants
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant ordinary steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST Р 51394 - 99 | 59.035–65.9 | < 0.4 | < 2 | 17–18.5 | < 0.3 | 14.5–16.5 | < 0.025 | < 0.03 | < 0.01 | 2.6–3.1 | < 0.1 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Sheet | GOST 51394-99 | 0.8–3.9 | 490–690 | 190 | 40 | |||
| The bar is hardened. | GOST 51394-99 | Ø 4–6 | 860–1100 | 690 | 12 |
Standards
| Standard | Description |
|---|---|
| GOST Р 51394 - 99 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| N | % | Nitrogen |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |