03H19G10N7M2
Weldability without restrictions.
for the manufacture of welded products, operating at temperatures ranging from 0 to -253 degrees.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Cryogenic structural steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Mo, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 4405-75 | 57.21–63.7 | < 0.8 | 9–11 | 18.5–20.5 | 6.5–7.5 | < 0.035 | < 0.03 | < 0.025 | 2–2.5 | 0.3–0.4 |
Information on suppliers
Technological Properties
| Weldability |
|---|
| no limits |
Standards
| Standard | Description |
|---|---|
| GOST 4405-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| N | % | Nitrogen |
Designation of types of weldability
| Parameter | Units of measurement | Description |
|---|---|---|
| no limits | Welding is performed without heating and without subsequent heat treatment | |
| Boundedly welded | Welding is possible with heating up to 100–120 °C and subsequent heat treatment | |
| Difficult to weld | For obtaining quality welded joints, additional operations are required: heating up to 200–300 °C for welding, heat treatment after welding — annealing | |
| Not applicable for welded structures |