03H20N65G5M4VB
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Ca, % | Mn, % | Cr, % | Ni, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Y, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 0.3 | < 0.2 | < 0.1 | 4–5 | 18–22 | 62.845–71 | < 0.1 | < 0.1 | < 0.015 | < 0.03 | < 0.01 | 2.2–3 | < 0.1 | 4–5 | 0.8–1.2 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ca | % | Calcium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Y | % | Yttrium |
| Mo | % | Molybdenum |
| W | % | Tungsten |