Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Zr, % |
Ce, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
ET, % |
| TU 14-1-3880-84 |
61.065–67.15 |
< 0.4 |
1–2 |
23.5–25 |
< 0.3 |
5.8–6.8 |
< 0.1 |
< 0.1 |
< 0.035 |
< 0.03 |
< 0.02 |
2.5–3.5 |
0.05–0.15 |
< 0.5 |
Information on suppliers
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Zr |
% |
Zirconium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |