05H12N6D2MFSGT
Hardness 05Х12Н6Д2МФСГТ heat treated (GOST 5950−2000): HB 10 -1 = 293 MPa
Tool shaping parts of molds molding of rubber and plastic products
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tool steel | Alloy tool steel |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Ca, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Zr, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 5950-73 | 73.35–79.99 | 0.6–1.2 | < 0.03 | < 0.03 | 0.2–1.2 | 11.5–13.5 | 0.4–0.8 | 1.4–2.2 | 5.5–6.5 | 0.2–0.5 | < 0.15 | < 0.03 | 0.01–0.08 | < 0.03 | 0.2–0.4 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 5950-73 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Ca | % | Calcium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| Zr | % | Zirconium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |