05H20N32TL
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 39.56–50.7475 | 0.0005–0.65 | 0.0005–0.74 | 19–23 | 0.25–0.6 | < 0.2 | 30–34 | 0.0005–0.1 | 0.0005–0.45 | < 0.03 | < 0.05 | < 0.02 | < 0.5 | 0.0005–0.1 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| BGH 4959 | RA 330 TX |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |