06HGSYU
for the manufacture of parts of cold plastic deformation
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Low alloy structural steel for welded structures |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-4554-88 | 96.58–98.28 | 0.3–0.6 | 1.1–1.4 | 0.3–0.6 | < 0.3 | < 0.3 | 0.02–0.07 | < 0.03 | < 0.09 | < 0.03 |
Information on suppliers
Mechanical properties at 20 °C
Standards
| Standard | Description |
|---|---|
| TU 14-1-4554-88 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |