08GDNF
For the manufacture of critical parts for shipbuilding and ship repair
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Alloyed structural steel |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | W, % |
|---|---|---|---|---|---|---|---|---|---|
| TU 108-11-514 - 80 | 0.15–0.4 | 0.6–1 | < 0.3 | 0.8–1.2 | 0.15–1.55 | < 0.035 | < 0.1 | < 0.04 | 0.05–0.15 |