08H14F
For the production of electric-welded pipes for the petrochemical industry; pipes for flue gas systems in motor vehicles.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| TU 14-159-249 - 94 | 82.965–86.85 | < 0.8 | < 0.8 | 13–15 | 0.15–0.3 | < 0.035 | < 0.08 | < 0.02 |