08H14MF (08H14MF-Sh)
For the manufacture of billets and strips intended for the production of pipes, boilers, steam pipes and manifolds with high and supercritical steam parameters, components and nuclear power engineering equipment and power station.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | V, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| TU 14-3-1808 - 91 | 82.695–85.6 | 0.2–0.45 | 0.8–1.2 | 13–14.8 | 0.15–0.3 | < 0.035 | 0.05–0.1 | < 0.02 | 0.2–0.4 |