08Х15Н5Д2Т-Ш (08H15N5D2T, EP410-Sh, VNS-2-Sh, EP410)
for the manufacture of parts of aviation equipment units; for the production of welding wire used for surfacing of parts and welding of metal structures in power engineering; for the manufacture of welding electrodes.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-3577 - 83 | 74.882–79.4 | < 0.7 | < 1 | 14–15 | 0.15–0.3 | 1.75–2.5 | 4.7–5.5 | < 0.02 | < 0.08 | < 0.018 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Tape softly. | TU 14-1-3577 - 83 | 980 | 785 | 8 | ||||
| The tape is hardcore. | TU 14-1-3577 - 83 | 1370 | 1275 | 5 | Aging 450oC, cooling air |
Standards
| Standard | Description |
|---|---|
| TU 14-1-3577 - 83 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |