0N9
vessels and devices working under pressure at temperatures up to -196 ° C
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Structural steel |
Cryogenic structural steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ni, % |
P, % |
C, % |
S, % |
| TU 14-105-846-2008 |
89.43–90.88 |
0.17–0.37 |
0.45–0.6 |
8.5–9.5 |
< 0.02 |
< 0.06 |
< 0.02 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$\psi$$, % |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Alloy |
|
|
|
|
720 |
520 |
28 |
82 |
2530 |
Double normalization with tempering |
| Alloy |
|
|
|
|
600 |
450 |
27 |
79 |
1960 |
Hardened and tempered |
Analogues
| Germany |
USA |
| G-X 8 Ni 9 |
X7Ni9 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$\psi$$ |
% |
Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |