10X11N23T3MR-VD
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 108.961.05-80 | 54.615–65.65 | < 0.6 | < 0.8 | < 0.75 | 10–12.5 | 2.6–3.2 | 21–25 | < 0.8 | < 0.025 | < 0.1 | < 0.01 | 0.75–1.6 |
Note: The maximum content of H in evacuated metal should be no more than 3 cm3 / 100g
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 108.961.05-80 | |
| TU 14-1-2902-80 | |
| TU 14-1-2918-80 | |
| TU 14-1-312-72 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |