10H2GNM (10X2GNMA)
It is used for welding of vessels. pressurized
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Alloyed structural steel |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| TU 108-11-928 - 87 | 0.17–0.37 | 0.9–1.3 | 0.9–2.3 | < 0.3 | 0.15–0.65 | < 0.03 | < 0.12 | < 0.03 | 0.45–0.65 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 108-11-928 - 87 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |