10H2M1
Sheets and strips GOST 10885−85;
Used as the base layer in the manufacture of hot-rolled two-layer corrosion-resistant sheets;
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Low alloy structural steel for welded structures |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10885-85 | 96.1–96.75 | 0.17–0.37 | 0.3–0.6 | 2–2.5 | < 0.6 | < 0.03 | 0.08–0.12 | < 0.03 | 0.9–1.1 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Sheet | GOST 10885-85 | 30–60 | 440 | 235 | 19 |
Standards
| Standard | Description |
|---|---|
| GOST 10885-85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |