10HGSN1D (SHL-45)
as the base layer in the manufacture of hot-corrosion-resistant double-layer sheet;
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Low alloy structural steel for welded structures |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10885-85 | 95.01–96.8 | 0.7–1 | 0.5–0.9 | 0.4–0.7 | 0.3–0.6 | 1.3–1.6 | < 0.035 | < 0.12 | < 0.035 |
Information on suppliers
Mechanical properties at 20 °C
Standards
| Standard | Description |
|---|---|
| GOST 10885-85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |