110G13FTL

Enclosure vortex and ball mills, crusher jaws, tram and railway switches and crossings, track shoe, stars, excavator bucket teeth and other parts operating at impact wear; the details of metallurgical and ore dressing oborudovaniya. Stal austenitic.

Classification

Country Section Category
CIS, Russia, Ukraine Steels and alloys for castings Steel for casting with special properties

Chemical composition

Standard Fe, % Si, % Mn, % Ti, % V, % P, % C, % S, %
GOST 977-88 82.78–87.09 0.4–0.9 11.5–14.5 0.01–0.05 0.1–0.3 < 0.12 0.9–1.3 < 0.05

Information on suppliers

Режимы термической обработки

Обработка
Закалка 1050 - 1100 ° C, охлаждение в воде

Standards

Standard Description
GOST 977-88

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Ti % Titan
V % Vanadium
P % Phosphorus
C % Carbon
S % Sulfur