11M5F (EP980)
The tool for processing carbon and structural steels.
For the manufacture of tools.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tool steel | High speed tool steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | V, % | Ce, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-2678-79 | 85.79–87.17 | < 0.5 | < 0.4 | 3.8–4.2 | < 0.4 | 1.3–1.6 | < 0.15 | < 0.03 | 1.02–1.1 | < 0.03 | 5.2–5.8 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 8300 |
Standards
| Standard | Description |
|---|---|
| TU 14-1-2678 - 0 | |
| TU 14-1-2678-79 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| V | % | Vanadium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |