11YUA
for clad strips by hot rolling; for cold-rolled strip intended for the manufacture of parts by deep drawing.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Carbonaceous quality structural steel |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 803 - 81 | < 0.13 | 0.3–0.5 | < 0.15 | < 0.2 | < 0.25 | 0.02–0.07 | < 0.025 | 0.08–0.13 | < 0.025 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|
| Tape | GOST 8851 - 75 | 290–410 | 28 |
Standards
| Standard | Description |
|---|---|
| GOST 803 - 81 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |