1230ph (VAD23pch)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Al, % |
Li, % |
Cd, % |
OE, % |
ET, % |
| OST 1 90026-80 |
< 0.15 |
< 0.1 |
< 0.03 |
0.4–0.8 |
0.03–0.15 |
4.8–5.8 |
< 0.1 |
91.12–93.77 |
0.9–1.4 |
0.1–0.25 |
< 0.05 |
< 0.05 |
Information on suppliers
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| OE |
% |
Other items |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Al |
% |
Aluminium |
| Li |
% |
Li |
| Cd |
% |
Cadmium |