12HN2MDF
Low alloy high strength steel used in shipbuilding
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Alloyed structural steel |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-3116 - 81 | 0.2–0.4 | 0.45–0.75 | 1.05–1.3 | 0.35–0.65 | 1.85–2.15 | < 0.03 | 0.09–0.13 | < 0.03 | 0.1–0.18 | 0.01–0.05 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-1-3116 - 81 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |