1310Sh (AD31Sh)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Al, % | Pb, % | As, % | OE, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 4784-97 | < 0.35 | 0.2–0.6 | 0.45–0.9 | < 0.1 | < 0.1 | < 0.1 | < 0.1 | < 0.1 | 97.285–99.35 | < 0.15 | < 0.015 | < 0.05 | < 0.15 |
Note: When used for anodizing: Fe <0.3
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| Alcron | 6083 |
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| OE | % | Other items |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |