1572
Hot-rolled sheet steel, designed for magnetic circuits of electrical machines
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Electrical steel | Sulfur Electrotechnical Steel |
Chemical composition
| Standard | Fe, % | Si, % |
|---|---|---|
| GOST 21427.3-75 | 95.2–96.2 | 3.8–4.8 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
|---|---|---|
| 20 | 7550 | 600 |
Magnetic properties
| Rolling | Dimensions, $$mm$$ | $$B_{100}$$, $$T$$ | $$B_{1000}$$, $$T$$ |
|---|---|---|---|
| Sheet hot rolled. | 0.35 | 0.87 | 1.3 |
Standards
| Standard | Description |
|---|---|
| GOST 21427.3-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
| $$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |
Description of magnetic properties
| Parameter | Units of measurement | Description |
|---|---|---|
| Dimensions | $$mm$$ | |
| $$B_{100}$$ | $$T$$ | Magnetic induction (not less) in a magnetic field while magnetic field strength is 100 A/m |
| $$B_{1000}$$ | $$T$$ | Magnetic induction (not less) in a magnetic field while magnetic field strength is 1000 A/m |