16X
For the magnetic cores of different management systems anchors and magnets; parts of electric machines without protective coatings, working in difficult conditions of exposure, temperature and pressure;
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precision alloys |
Soft Magnetic Precision Alloys |
Chemical composition
| Standard |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
| GOST 10994-74 |
< 0.2 |
< 0.3 |
15.5–16.5 |
< 0.3 |
< 0.015 |
< 0.015 |
< 0.015 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
220 |
|
7750 |
0.44 |
| 100 |
|
9.9 |
|
|
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$\psi$$, % |
Treatment |
| Tape |
|
|
|
|
250 |
196 |
25 |
63 |
|
| Tape |
|
|
|
cold-work |
390 |
|
5 |
|
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Tape |
|
cold-work |
185 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$\psi$$ |
% |
Reduction in cross section on fracture |