1903 (ABT102)
For the production of flat bars
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Zr, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1-92014 - 90 | < 0.35 | < 0.25 | 0.0002–0.003 | 2.1–2.6 | 0.05–0.15 | 0.12–0.25 | 0.03–0.1 | < 0.2 | 4.7–5.3 | 0.07–0.12 | 90.677–92.9298 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| OST 1-92014 - 90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |