1980
For the manufacture of pipes and extruded profiles; parts of special branches of mechanical engineering and shipbuilding and aeronautics.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Zr, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|---|
| OST 5.9466 - 88 | < 0.3 | < 0.2 | 2–2.6 | 0.3–0.5 | 0.1–0.2 | < 0.07 | < 0.08 | 4–4.8 | 0.1–0.18 | 91.07–93.5 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 2760 |
Standards
| Standard | Description |
|---|---|
| OST 5.9466 - 88 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Zr | % | Zirconium |
| Al | % | Aluminium |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |