2012
Thin-sheet cold rolled grain oriented steel, designed for magnetic circuits of electrical machinery, apparatus and appliances
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Electrical steel |
Sulfur Electrotechnical Steel |
Chemical composition
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
7850 |
140 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Sheet |
GOST 21427.2-83 |
|
|
cold rolling |
290–490 |
15–35 |
|
Magnetic properties
| Rolling |
Dimensions, $$mm$$ |
$$P_{1.0/50}$$, $$W/kg$$ |
$$P_{1.5/50}$$, $$W/kg$$ |
$$B_{1000}$$, $$T$$ |
$$B_{2500}$$, $$T$$ |
$$B_{5000}$$, $$T$$ |
$$B_{10000}$$, $$T$$ |
$$B_{30000}$$, $$T$$ |
| Sheet cold rolled. |
0.65 |
3.6 |
8 |
1.5 |
1.62 |
1.72 |
1.82 |
2.02 |
| Sheet cold rolled. |
0.5 |
2.9 |
6.5 |
1.5 |
1.62 |
1.72 |
1.82 |
2.02 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
Description of magnetic properties
| Parameter |
Units of measurement |
Description |
| Dimensions |
$$mm$$ |
|
| $$P_{1.0/50}$$ |
$$W/kg$$ |
Specific magnetic losses (no more) while the magnetic induction is 1.0 T and frequency is 50 Hz |
| $$P_{1.5/50}$$ |
$$W/kg$$ |
Specific magnetic losses (no more) while the magnetic induction is 1.5 T and frequency is 50 Hz |
| $$B_{1000}$$ |
$$T$$ |
Magnetic induction (not less) in a magnetic field while magnetic field strength is 1000 A/m |
| $$B_{2500}$$ |
$$T$$ |
Magnetic induction (not less) in a magnetic field while magnetic field strength is 2500 A/m |
| $$B_{5000}$$ |
$$T$$ |
Magnetic induction (not less) in a magnetic field while magnetic field strength is 5000 A/m |
| $$B_{10000}$$ |
$$T$$ |
Magnetic induction (not less) in a magnetic field while magnetic field strength is 10000 A/m |
| $$B_{30000}$$ |
$$T$$ |
Magnetic induction (not less) in a magnetic field while magnetic field strength is 30000 A/m |