20H14
For the production of hot-rolled and cold-drawn wire, designed for mechanized arc surfacing.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Alloyed structural steel |
Chemical composition
| Standard | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|
| GOST 10543 - 98 | < 0.8 | < 0.8 | 13–15 | < 0.6 | < 0.3 | 0.16–0.25 | < 0.25 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10543 - 98 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |