2215
Thin-sheet cold rolled grain oriented steel, designed for magnetic circuits of electrical machinery, apparatus and appliances
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Electrical steel | Sulfur Electrotechnical Steel |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
|---|---|---|
| 20 | 7750 | 250 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|
| Sheet cold rolled. | GOST 21427.2-83 | 300–450 | 20–35 |
Magnetic properties
| Rolling | Dimensions, $$mm$$ | $$B_{1000}$$, $$T$$ | $$B_{5000}$$, $$T$$ | $$B_{10000}$$, $$T$$ |
|---|---|---|---|---|
| Sheet cold rolled. | 0.5 | 1.53 | 1.72 | 1.8 |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
| $$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
Description of magnetic properties
| Parameter | Units of measurement | Description |
|---|---|---|
| Dimensions | $$mm$$ | |
| $$B_{1000}$$ | $$T$$ | Magnetic induction (not less) in a magnetic field while magnetic field strength is 1000 A/m |
| $$B_{5000}$$ | $$T$$ | Magnetic induction (not less) in a magnetic field while magnetic field strength is 5000 A/m |
| $$B_{10000}$$ | $$T$$ | Magnetic induction (not less) in a magnetic field while magnetic field strength is 10000 A/m |