23H2NVFA (EI659)
for the manufacture of rolled products used in the heat-treated
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Alloyed structural steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 11268 - 76 | 92.91–95.46 | 0.17–0.37 | 0.3–0.7 | 1.9–2.4 | < 0.03 | < 0.25 | 0.8–1.2 | 0.18–0.28 | < 0.025 | 0.19–0.26 | < 0.025 | < 0.15 | 1–1.4 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | $$\psi$$, % | $$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|---|---|
| Rod | TU 14-1-950-74 | 1130 | 930 | 50 | 540 | 12 | Hardening and tempering | |||
| The plates | GOST 11269-76 | 490–780 | 17 | Normalization | ||||||
| The plates | GOST 11269-76 | 1130 | 390 | 9 | Hardening and tempering | |||||
| Sheet | GOST 11268 - 76 | 490–780 | 17 | Normalization | ||||||
| Sheet | GOST 11268 - 76 | 1130 | 9 | Hardening and tempering |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| The plates | GOST 11269-76 | normalization | 170–241 |
Standards
| Standard | Description |
|---|---|
| GOST 11268 - 76 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\psi$$ | % | Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |