27HGSNMDTL (27HGSNMDTLA)
tips for frozen soil rippers, bulldozers heavy support rollers, drive pinion, sprockets tracked vehicles and other items.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Steels and alloys for castings | Steel for casting with special properties |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | РЗЭ, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 21357-87 | 93.43–96.33 | 0.7–1.3 | 0.9–1.5 | 0.7–1.3 | 0.03–0.07 | 0.3–0.5 | 0.7–1.2 | 0.02–0.05 | < 0.02 | 0.22–0.31 | < 0.02 | 0.1–0.3 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | $$\psi$$, % | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|---|
| Castings | GOST 21357-87 | 800 | 650 | 20 | 12 | Normalization 910 - 930 ° C, Vacation 590 - 610 ° C | |||
| Castings | GOST 21357-87 | 850 | 700 | 25 | 12 | Water hardening 910 - 930 ° C, Release 640 - 660 ° C | |||
| Castings | GOST 21357-87 | 1400 | 1150 | 12 | 8 | Water hardening 910 - 930 ° C, Release 200 - 220 ° C, (wear-resistant steel) |
Heat Treatment Modes
| Treatment |
|---|
| Normalization 910 - 930 ° C, Vacation 590 - 610 ° C |
| Water hardening 910 - 930 ° C, Release 640 - 660 ° C |
| Water hardening 910 - 930 ° C, Release 200 - 220 ° C, (wear-resistant steel) |
Analogues
| Germany | USA |
|---|---|
| 30 Mn 5 | 1330 |
Standards
| Standard | Description |
|---|---|
| GOST 21357-87 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| РЗЭ | % | Rare earth elements |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\psi$$ | % | Reduction in cross section on fracture |