3421
The chemical composition is not standardized .
cold rolled anisotropic tape designed for magnetic circuits of electrical machines and instruments
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Electrical steel |
Sulfur Electrotechnical Steel |
Chemical composition
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
7650 |
500 |
Magnetic properties
| Rolling |
Dimensions, $$mm$$ |
$$B_{1000}$$, $$T$$ |
$$B_{2500}$$, $$T$$ |
| Sheet cold rolled. |
0.2 |
1.45 |
1.7 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of magnetic properties
| Parameter |
Units of measurement |
Description |
| Dimensions |
$$mm$$ |
|
| $$B_{1000}$$ |
$$T$$ |
Magnetic induction (not less) in a magnetic field while magnetic field strength is 1000 A/m |
| $$B_{2500}$$ |
$$T$$ |
Magnetic induction (not less) in a magnetic field while magnetic field strength is 2500 A/m |