Precision alloy 35KH4F
- Chemical composition
| V | Vanadium | 3.5 — 4.5 |
| Fe | Iron | Rest |
| Co | Cobalt | 34.3 — 35.8 |
| Si | Silicon | <0.3 |
| Mn | Manganese | <0.4 |
| S | Sulfur | <0.02 |
| C | Carbon | <0.06 |
| P | Phosphorus | <0.02 |
| Cr | Chromium | 7.5 — 8.5 |
for the active part of the hysteresis motors
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Magnetic Hard Precision Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | 50.4–54.7 | < 0.3 | < 0.4 | 34.3–35.8 | 7.5–8.5 | 3.5–4.5 | < 0.02 | < 0.06 | < 0.02 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |