Nickel alloy with cobalt and chromium alloyed with molybdenum 35H32KXM
- Chemical composition
| Fe | Iron | <1.0 |
| Co | Cobalt | 31.0 — 33.0 |
| Si | Silicon | <0.15 |
| Mn | Manganese | <0.15 |
| Mo | Molybdenum | 9.0 — 10.5 |
| Ni | Nickel | 33.0 — 37.0 |
| S | Sulfur | <0.01 |
| Ti | Titanium | <1.0 |
| C | Carbon | <0.025 |
| P | Phosphorus | <0.015 |
| Cr | Chromium | 19.0 — 21.0 |
By agreement: Si + Mn <0.40
Analogs in Germany
MP 35 N
2.4999
Analogs in the USA
Allvac MP 35 N
MP 35 N Multiphase
Allvac 35 N
5758 E AMS
5844 D AMS
5845 D AMS
5758 F AMS
5844 E AMS
5845 E AMS
5758 AMS
5844 AMS
5845 AMS
AS7468 AMS
F 1636 (R 30035) ASTM F1636
F 2005 (R 30035) ASTM F2005
F 2068 (R 30035) ASTM F2068
F 2527 (R 30035) ASTM F2527
F 562 (R30035) ASTM F562
F 688 (R30035) ASTM F688
F 961 (R30035) ASTM F961
Carpenter MP35N Alloy Carpenter
MP35N Latrobe
MR0175 NACE
718 NACE Rolled Alloys
MP35N SPS
R30035 UNS
International equivalent — SY 35N ArcelorMittal
Production in Russia is carried out in accordance with the standards of GOST R 51396−99. The alloy is used for connecting force and implantable elements of products for the bones of the body.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST Р 51396 - 99 | < 1 | < 0.15 | < 0.15 | 31–33 | 19–21 | < 1 | 33.15–41 | < 0.015 | < 0.025 | < 0.01 | 9–10.5 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Wire heat treatment. | GOST 51396-99 | 800 | 300 | 40 | ||||
| The wire is half-worked. | GOST 51396-99 | 1000 | 650 | 20 | ||||
| Wire is hardened. | GOST 51396-99 | 1200 | 1000 | 10 |
Analogues
| USA |
|---|
| Allvac MP 35 N |
Standards
| Standard | Description |
|---|---|
| GOST Р 51396 - 99 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |