36G2SR
Production of hot-rolled special profile for earthmoving machinery blades
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Alloyed structural steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-136-348 - 2002 | 96.0791–97.6799 | 0.5–0.8 | 0.0001–0.0009 | 1.5–1.8 | < 0.25 | < 0.3 | < 0.3 | < 0.035 | 0.32–0.4 | < 0.035 |
Information on suppliers
Brinell hardness number
Standards
| Standard | Description |
|---|---|
| TU 14-136-348 - 2002 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |