Structural steel alloy 36KNM
- Chemical composition
| C | Carbon | <0.03 |
| Si | Silicon | <0.4 |
| Mn | Manganese | <0.5 |
| P | Phosphorus | <0.015 |
| S | Sulfur | <0.015 |
| Mo | Molybdenum | 2.8 — 3.2 |
| Ni | Nickel | 21.5 — 22.5 |
| Co | Cobalt | 35.5 — 37.0 |
| Fe | Iron | Rest |
For magnetic cores operating in sea water; Steel has high induction in weak and medium fields and low coercive force; with high corrosion resistance in sea water.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Soft Magnetic Precision Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | 36.34–40.2 | < 0.4 | < 0.5 | 35.5–37 | 21.5–22.5 | < 0.015 | < 0.03 | < 0.015 | 2.8–3.2 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
|---|---|---|
| 20 | 8200 | 0.48 |
Mechanical properties at 20 °C
Brinell hardness number
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
| $$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
| $$\psi$$ | % | Reduction in cross section on fracture |