An alloy based on iron alloyed with chromium and nickel. Contains titanium, molybdenum and aluminum (as a deoxidant) 36НХТЮ8М (EP52)
- Chemical composition
| Al | Aluminum | 1.0 — 1.3 |
| Fe | Iron | Rest |
| Si | Silicon | 0.3 — 0.7 |
| Mn | Manganese | 0.8 — 1.2 |
| Mo | Molybdenum | 7.5 — 8.5 |
| Ni | Nickel | 35.0 — 37.0 |
| S | Sulfur | <0.02 |
| Ti | Titanium | 2.7 — 3.2 |
| C | Carbon | <0.05 |
| P | Phosphorus | <0.02 |
| Cr | Chromium | 12.0 — 13.5 |
36NHTYUM8
EP52 (TU 14−1-279−72)
36NHTYUM8 (TU 14−1-279−72)
Heat resistant, corrosion resistant alloy. It is made in Russia in accordance with GOST 10994−74, and is intended for the manufacture of elastic sensitive elements operating at temperatures up to 400 degrees. WITH
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | With preset elastic properties |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | 34.51–40.7 | 0.3–0.7 | 0.8–1.2 | 12–13.5 | 2.7–3.2 | 35–37 | 1–1.3 | < 0.02 | < 0.05 | < 0.02 | 7.5–8.5 |
Information on suppliers
Mechanical properties at 20 °C
Brinell hardness number
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |