38NKD (38NKD-VI)
For vacuum tight junctions with glass, sapphire.
for vacuum junctions with glass U-6, S72−4; 1000000 * TFLE at temperatures ranging from -60 to +400 ºC less than 7.0−7.8 [1 / ºC]
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precision alloys |
With given TCLE |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
| GOST 10994-74 |
49.72–53.5 |
< 0.3 |
< 0.4 |
4.5–5.5 |
4.5–5.5 |
37.5–38.5 |
< 0.015 |
< 0.05 |
< 0.015 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
150 |
8200 |
0.5 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
|
|
|
|
|
450–550 |
23 |
Annealing |
Casting and technological parameters
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |