40gr
To improve the production of after — rivets critical applications; after carburizing or cyanidation — piston pin, friction disc spring fingers, the cam rollers, bolts, nuts, screws, gears, worms and other parts with high surface hardness and wear resistance; without heat treatment — welding the sub-frames, shoes, scarves, fittings, plugs; The track link of tractors.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Alloyed structural steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 4543-71 | 97.205–98.759 | 0.17–0.37 | 0.001–0.005 | 0.7–1 | < 0.3 | < 0.3 | < 0.3 | < 0.035 | 0.37–0.45 | < 0.035 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{P}$$, $$MPa$$ | $$\epsilon_L$$, % | $$\psi$$, % | $$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ | Treatment |
|---|---|---|---|---|---|---|---|---|---|---|
| Rod | GOST 4543-71 | 25 | 590 | 355 | 17 | 45 | 590 | Tempering 860 ° C, air Accommodation 600 ° C, air |
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| Alloy | GOST 4543-71 | 207 |
Analogues
| USA | Germany |
|---|---|
| G10430 | 1.1157 (40Mn4) |
Standards
| Standard | Description |
|---|---|
| GOST 4543-71 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
| $$\psi$$ | % | Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |