40HGNM
Parts of auxiliary units of machines and devices; Car chassis parts
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Structural steel |
Alloyed structural steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| GOST 4543-71 |
95.78–97.51 |
0.17–0.37 |
0.5–0.8 |
0.6–0.9 |
< 0.3 |
0.7–1.1 |
< 0.035 |
0.37–0.43 |
< 0.035 |
0.15–0.25 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Rod |
GOST 4543-71 |
25 |
|
|
980 |
835 |
12 |
880 |
Tempering 840 ° C, oil, Holidays 560-620 ° C, air |
Analogues
| Germany |
USA |
| 40NiCrMo22 |
G98400 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |