40HN2VA (40XNVA)
For the manufacture crankshafts responsible bolts and other fasteners, special fasteners and other heavy-duty components; azotiruemyh parts of aircraft construction.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Structural steel | Alloyed structural steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-950-74 | 94.11–96.31 | 0.17–0.37 | 0.5–0.8 | 0.6–0.9 | < 0.03 | < 0.25 | 1.25–1.65 | < 0.05 | < 0.025 | 0.37–0.44 | < 0.025 | < 0.15 | 0.8–1.2 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | $$\psi$$, % | $$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|---|---|
| Rod | TU 14-1-950-74 | Ø 25 | 980–1080 | 835–930 | 50–55 | 785–980 | 12 | Hardening and tempering |
Standards
| Standard | Description |
|---|---|
| TU 14-1-950-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\psi$$ | % | Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |