Multicomponent alloy based on iron 40KNHMVTYU
- Chemical composition
| Al |
Aluminum |
0.2 — 0.5 |
| W |
Tungsten |
6.0 — 7.0 |
| Fe |
Iron |
Rest |
| Co |
Cobalt |
39.0 — 41.0 |
| Si |
Silicon |
<0.5 |
| Mn |
Manganese |
1.8 — 2.2 |
| Mo |
Molybdenum |
3.0 — 4.0 |
| Ni |
Nickel |
18.0 — 20.0 |
| S |
Sulfur |
<0.02 |
| Ti |
Titanium |
1.5 — 2.0 |
| C |
Carbon |
<0.05 |
| P |
Phosphorus |
<0.02 |
| Cr |
Chromium |
11.5 — 13.0 |
Domestic analogue — EP4
for wrist watch springs. Technical requirements — according to GOST 10994−74 and GOST 14118−85
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precision alloys |
With preset elastic properties |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| GOST 10994-74 |
9.71–19 |
< 0.5 |
1.8–2.2 |
39–41 |
11.5–13 |
1.5–2 |
18–20 |
0.2–0.5 |
< 0.02 |
< 0.05 |
< 0.02 |
3–4 |
6–7 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
Treatment |
| Wire |
|
|
|
cold-work |
1470 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |