Precision iron-nickel alloy 42NHTY
- Chemical composition
| Al | Aluminum | 0.5 — 1.0 |
| Fe | Iron | Rest |
| Si | Silicon | 0.5 — 0.8 |
| Mn | Manganese | 0.5 — 0.8 |
| Ni | Nickel | 41.5 — 43.5 |
| S | Sulfur | <0.02 |
| Ti | Titanium | 2.4 — 3.0 |
| C | Carbon | <0.05 |
| P | Phosphorus | <0.02 |
| Cr | Chromium | 5.3 — 5.9 |
N41XT
H41XTA
42NHTUA
Analogs in the USA
902
NI-SPAN C-902
5223 D AMS
5225 D AMS
5221 D AMS
5223 E AMS
5221 AMS
5223 AMS
5225 AMS
NI-SPAN alloy C-902 Special Metals
N09902 UNS
K70640 UNS
for elastic sensitive elements operating at temperatures up to 100 degrees. C Technical requirements — according to GOST 10994−74 The alloy is also included in the following standards: Standard Name GOST 14117−85 Tape made of precision alloys for elastic elements. Technical conditions GOST 14118−85 Precision alloy wire for elastic elements. Technical conditions GOST 14119−85 Bars from precision alloys for elastic elements. Technical conditions
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | With preset elastic properties |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | 44.91–49.3 | 0.5–0.8 | 0.5–0.8 | 5.3–5.9 | 2.4–3 | 41.5–43.5 | 0.5–1 | < 0.02 | < 0.05 | < 0.02 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$E\cdot 10^{9}$$, $$MPa$$ | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
|---|---|---|
| 20 | 182 | 9.5 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{P}$$, $$MPa$$ | $$\epsilon_L$$, % | $$\psi$$, % | Treatment |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | 1180–1570 | ||||||||
| Round | 980 | 635 | 8 | 25 | Quenching and aging | ||||
| Wire | cold-work, half-load | 980 | |||||||
| Wire | cold-work | 1080 | |||||||
| Tape | cold-work | 830 |
Brinell hardness number
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$E\cdot 10^{9}$$ | $$MPa$$ | Elastic modulus |
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
| $$\psi$$ | % | Reduction in cross section on fracture |